The immersion environment in engineering terms
A seawater exposure is not simply "wet". Its three dominant effects on a composite are water absorption, salt-assisted degradation and electrochemical interaction with the protection system.
Seawater diffuses into a thermoset laminate slowly, but it also carries ions. The salt does not permeate at the same rate as the water, so the outer layer can end up with a different local concentration than the interior, generating an osmotic driving force that leads to blistering - the same mechanism that affects boat hulls, made more severe here because the structure cannot be hauled out and dried.
Under permanent immersion the resin also sees biological activity: bacterial and algal growth on the surface can alter local water chemistry, and the surface biofouling layer is abrasive during cleaning operations. Combined with sand and current-driven particle abrasion, this erodes any unprotected laminate surface over time, which makes a properly cured, resin-rich outer layer a durability requirement rather than a cosmetic one.
The electrochemical environment is unique to offshore structures. Sacrificial anodes maintain a cathodic potential on the steel they protect, and that potential can generate hydroxyl ions at the metal surface. If a resin coating or laminate is bonded to steel and is exposed to that environment, cathodic disbondment can cause the coating to lose adhesion. Formulating for that condition usually means a high cross-link-density resin with excellent wet adhesion, and a surface preparation designed for it.