Process sequence and resin demands at each stage
A CIPP resin is specified against the whole installation sequence, because a perfect cured property is meaningless if the liner cannot be impregnated or delivered to position.
1. Impregnation (wet-out)
The liner is saturated in the factory or at a wet-out facility. The resin must have a viscosity low enough to fully penetrate a felt or glass-fibre liner within the process time, and a working life long enough to handle a large diameter liner without gelation. Void content left by incomplete impregnation is the single biggest cause of low flexural modulus and long-term leakage in CIPP.
2. Load-in and inversion/pull-in
The impregnated liner is transported and installed, then inverted or pulled into the host pipe. During this stage the liner is largely unconstrained and under tension; it must retain its resin without draining under gravity, and the resin must be tolerant of a delay between wet-out and cure.
3. Curing
Thermal curing uses hot water, steam or, in UV-cure systems, a light train pulled through the liner. Each method imposes a different requirement: thermal cure depends on heat transfer through the liner and around the pipe circumferentially, which is difficult in large diameters and in thick liners; UV cure needs a photoinitiator system that cures through the full wall thickness and a translucent liner so the light penetrates.
4. Inspection and reinstatement
After cure, the ends are cut and the liner is inspected, usually by CCTV for wall thickness and seam integrity, and the pipe is returned to service through lateral connections cut into the liner wall.