FGD Liner Resin for Power Plant Stack Liners

A flue-gas desulphurisation stack liner is one of the most hostile duty cycles in industrial composites: hot acidic condensate, particulate abrasion, thermal cycling and, in a wet stack, the risk of acid attack from the sulphuric acid dew point upward.

Understanding the FGD duty cycle

The resin is asked to survive a service that moves continuously between three failure-driving conditions.

Untreated flue gas contains sulphur dioxide; the FGD process scrubs it with an alkaline slurry and produces a saturated, humid gas stream with a residual acid content. The gas leaves the scrubber close to its adiabatic saturation temperature and flows up the stack, where it cools against the stack wall. Once the wall temperature drops below the acid dew point, acidic condensate forms on the surface - and that condensate is both hot and chemically aggressive, typically dominated by sulphuric acid with some nitric and hydrochloric acid contributions.

The second driver is thermal cycling. On plant start-up the stack liner warms from ambient to full operating temperature over a few hours; on shutdown it cools back. If the liner is on steel or concrete, the parent structure expands at a different rate from the laminate, so every cycle imposes a shear and bending load on the bond between them. A resin with low elongation cannot survive this for a typical plant life of 25-30 years.

The third driver is abrasion. Particulate matter, and in some plants gypsum dust carried over from the scrubber, impinges on the internal surface at the highest velocities in the system. The protection here is not only resin choice but surface finish and, where required, a reinforced wear layer.

Why novolac vinyl ester is the FGD standard

The chemistry of hot concentrated sulphuric acid narrows the viable resin set very sharply, and novolac vinyl ester is the usual answer for the most severe sections.

Sulphuric acid at elevated temperature attacks ester linkages by hydrolysis. The rate is sensitive to both acid concentration and temperature, and it accelerates dramatically above roughly 50 °C for concentrated acid. Ordinary isophthalic polyester is unsuitable for the hot condensate duty, and even standard bisphenol-A vinyl ester has limited margin at the highest temperatures reached in an undiluted wet stack.

Novolac (phenol novolac) epoxy vinyl ester has a higher aromatic content and a denser cross-link network than bisphenol-A vinyl ester. The result is superior resistance to concentrated acids and oxidising media, and a higher HDT. Its lower elongation is a real trade-off, which is why it is often used as the chemical barrier within a laminate whose structural layers use a tougher vinyl ester, rather than as a monolithic novolac lay-up.

Where the acid duty is combined with high particulate abrasion or where the liner will be chemically cleaned, a flake-glass or ceramic-filled barrier layer is common. Flake glass creates a tortuous diffusion path and resists permeation; the barrier function is more important than adding thickness to the structural layer.

Typical material assignment by stack zone

Upper stack (below acid dew point, continuous condensate)Novolac vinyl ester barrier, BPA vinyl ester structure
Transition / inlet zone (highest temperature)Novolac vinyl ester, higher HDT grade
Ducting upstream of the stackBPA vinyl ester, with novolac where condensate is expected
Exit duct and chimney capFlake-glass or ceramic-filled wear barrier on BPA vinyl ester

Standards and qualification testing

  • ASTM C581: chemical resistance of thermosetting resins used in glass-fibre-reinforced structures - the standard immersion test that produces flexural property retention against time.
  • ASTM D3681: chemical resistance of thermosetting resins in a deflecting environment (the 1/8-inch bar test), which correlates with resistance to stress-corrosion cracking in service.
  • ASTM C582 / C1310 for hand lay-up contact-moulded laminates and for the quality of applied linings.
  • ASTM D790: flexural strength and modulus, the primary structural property for liner design.
  • ASTM D2583 / D2240 for hardness and cure verification before the lining is closed up.
  • ASTM D4541: pull-off adhesion test for the bond to a steel or concrete substrate, essential given thermal cycling.
  • Air-permeability or spark (holiday) testing of the finished lining to find pinholes that would let condensate reach the steel behind it.

Design and installation considerations

Most FGD lining failures are installation failures that a more expensive resin cannot rescue, so the specification has to cover the process as carefully as the chemistry.

  • The liner thickness and the structural design should be separated: the barrier layer is sized for chemical and permeation resistance, the structural layer for the differential thermal strain. Simplified "single-thickness" specifications are a common source of premature cracking.
  • Steel substrates must be prepared by an approved method (typically abrasive blast to a specified cleanliness grade) and primed within the recoat window; the primer chemistry must be compatible with the vinyl ester, not chosen independently.
  • Exotherm control in thick spray or hand lay-up sections is critical: an uncontrolled exotherm can scorch the resin, and the damaged material may not be visible from the finished surface.
  • The lining must be continuous around nozzles, manways, expansions and instrument penetrations; every discontinuity is where acid reaches the substrate.
  • Repair procedures and a defined inspection criterion (spark testing plus adhesion spot checks) are part of a workable specification.

Failure modes seen in service

  • Acid attack at the condensate line: a novolac barrier is required where BPA vinyl ester was specified.
  • Through-thickness cracking at stiffener connections: differential thermal expansion and stress concentration, addressed by geometry and a higher-elongation structural resin.
  • Bond failure between the lining and the stack shell: usually a surface preparation or contamination issue rather than a resin issue.
  • Wear-through where particulate velocity is highest: needs a wear-resistant top layer, not a thicker structural laminate.
  • Blistering after wet/dry cycling on shutdown: cure quality and barrier thickness determine the risk.

Key Screening Properties for FGD Stack Liners

Screening values for fgd stack liners service - check them against the service temperature and medium before specifying.

Base Chemistry
Novolac Vinyl Ester
HDT
130 - 150°C
Tensile Elongation
2.5 - 3.5%
Viscosity (25°C)
400 - 600 mPa·s

Recommended Grades for FGD Stack Liners

LC-9007

Novolac VE

The industry benchmark for FGD lining systems.

View Technical Details
LC-9001S

Standard VE

Used for less aggressive ducting sections.

View Technical Details

FGD Stack Liners Technical FAQ

Short answers on the points that decide a specification.

Can this be sprayed?

Yes, we provide spray-grade Novolac resins for faster internal lining of large stacks.

How does it handle thermal cycling?

Our rubber-modified Novolac versions provide the flexibility needed for expansion/contraction.

Related Applications

Other industries and processes that use similar Lechi resin systems.

Industrial & Infrastructure

Industrial Centrifugal Fans

Industrial & Infrastructure

Rail Transportation Interiors

Marine & Water Infrastructure

Marine Hulls & Decks

Marine & Water Infrastructure

Industrial Cooling Towers

Chemical & Heavy Industry

Chemical Pipes & Tanks

Transport & Aerospace

Automotive Body Panels

View all applications →

Request Quote & Samples for FGD Stack Liners

Send the process, service conditions and volume. We will reply with a grade recommendation, technical data and sample options.

Minimum 10 characters. Be specific about your requirements for better assistance.
By submitting this form, you acknowledge that your information will be processed according to our privacy policy. We typically respond within 24 hours during business days.